PENETRATION GRADE – EN
. | Test Method |
PENETRATION GRADE - EN |
|||||||
30/45 | 35/50 | 40/60 | 50/70 | 70/100 | 100/150 | 160/220 | 250/300 | ||
Penetration at 25°C | IP 49 | 30-45 | 35-50 | 40-60 | 50-70 | 70-100 | 100-150 | 160-220 | 250-300 |
Softening point °C | IP 58 | 52-60 | 50-58 | 48-56 | 46-54 | 43-51 | 39-47 | 35-43 | 30-38 |
Resistance to hardening at 163°C
- change of mass % (max.) – retained penetration (min.) - softening point after hardening, minimum (°C) |
IP 460 part 1 or IP 460 part 3 IP 49 IP 58 |
0.5 53 54 |
0.5 53 52 |
0.5 50 49 |
0.5 50 48 |
0.5 50 45 |
0.8 46 45 |
1.0 37 37 |
1.0 35 32 |
Flash point, minimum (°C) | IP 36 | 240 | 240 | 230 | 230 | 230 | 230 | 220 | 220 |
Solubility, minimum (%) | IP 47 | 99.0 | 99.0 | 99.0 | 99.0 | 99.0 | 99.0 | 99.0 | 99.0 |
Kinematic viscosity at 135°C, minimum (mm²/s) | IP 319 | 400 | 370 | 325 | 295 | 230 | 175 | 135 | 100 |